PDF下载 分享
[1]程方杰,等.直接埋藏法修补疲劳裂纹缺陷的研究[J].天津大学学报(自然科学与工程技术版),2020,53(05):502-507.[doi:10.11784/tdxbz201904064]
 Cheng Fangjie,Kong Kangqian,et al.Repair of Fatigue Crack Defects by Direct Burial Method[J].Journal of Tianjin University(Science and Technology),2020,53(05):502-507.[doi:10.11784/tdxbz201904064]
点击复制

直接埋藏法修补疲劳裂纹缺陷的研究

参考文献/References:

[1] Rodríguez-Sánchez J E,Dover W D,Brennan F P. Application of short repairs for fatigue life exten-sion[J]. International Journal of Fatigue,2004,26(4):413-420.

[2] Ayatollahi M R,Razavi S M J,Chamani H R. Fatigue life extension by crack repair using stop-hole technique under pure mode-Ⅰ and pure mode-Ⅱ loading condi-tions[J]. Procedia Engineering,2014,74:18-21.

[3] Rodríguez-Sánchez J E,Dover W D,Brennan F P,et al. Fracture mechanics analysis of fatigue crack re-paired joints[J]. Journal of Offshore Mechanics and Arctic Engineering,2005,127(2):182-189.

[4] 李冬霞,贾宝春,周金锁. 多次补焊对T型焊接接头疲劳强度的影响[J]. 中原工学院学报,2005,16(2):64-65.

Li Dongxia,Jia Baochun,Zhou Jinsuo. The effect of multiple reparing weld on T-shape joints weld bead fa-tigue strength[J]. Journal of Zhongyuan Institute of Technology,2005,16(2):64-65(in Chinese).

[5] 刘海涛,柳春图,黎之奇,等. 海洋平台用高强度钢多次补焊的疲劳分析[J]. 机械强度,2002,24(3):433-435.

Liu Haitao,Liu Chuntu,Li Zhiqi,et al. Fatigue anly-sis of multiple repairing welding on high strength off-shore structure steel[J]. Journal of Mechanical Strength,2002,24(3):433-435(in Chinese).

[6] 王志杰,齐芳娟,林 松,等. 焊补对SMA490BW焊接接头疲劳性能的影响[J]. 焊接学报,2015,36(5):109-112.

Wang Zhijie,Qi Fangjuan,Lin Song,et al. Effect of repair welding on fatigue properties of SMA490BW steel welded joints[J]. Transactions of the China Weld-ing Institution,2015,36(5):109-112(in Chinese).

[7] 傅利斌,许鸿吉,董 强,等. 补焊次数对S355J2W+N低合金钢T型接头疲劳性能和组织的影响[J]. 大连交通大学学报,2017,38(5):75-78.

Fu Libin,Xu Hongji,Dong Qiang,et al. Effect of repair welding times on fatigue properties and micro-structure of S355J2W+N low alloy steel T welding joints[J]. Journal of Dalian Jiaotong University,2017,38(5):75-78(in Chinese).

[8] 吴晓明,张艳辉,钮旭晶,等. 补焊道次对Q345B低合金钢焊接接头疲劳性能的影响[J]. 机械工程材料,2012,36(11):69-71.

Wu Xiaoming,Zhang Yanhui,Niu Xujing,et al. Ef-fects of repairing welding passes on fatigue property of butt joints of Q345B low-alloy steel[J]. Materials for Mechanical Engineering,2012,36(11):69-71(in Chinese).

[9] Akyel A,Kolstein M H,Bijlaard F S K. Fatigue strength of repaired welded connections made of very high strength steels[J]. Engineering Structures,2018,161:28-40.

[10] Rodríguez-Sánchez J E,Rodríguez-Castellanos A,Pérez-Guerrero F,et al. Offshore fatigue crack repair by grinding and wet welding[J]. Fatigue & Fracture of Engineering Materials & Structures,2011,34(7):487-497.

[11] 薛 彬,张天会,徐人平,等. 残余压应力场对 B780CF 钢焊接接头疲劳裂纹扩展的影响[J]. 焊接学报,2016,37(6):103-108.

Xue Bin,Zhang Tianhui,Xu Renping,et al. Effect of residual compressive stress field on fatigue crack growth of B780CF steel welded joints[J]. Transactions of the China Welding Institution,2016,37(6):103-108(in Chinese).

[12] 张世伟,陈学德,张 勇,等. 秦山核电厂稳压器管嘴DMW焊缝堆焊修复残余应力分析[J]. 核动力工

程,2016(增2):7-9.

Zhang Shiwei,Chen Xuede,Zhang Yong,et al. Analysis of weld overlay residual stress for dissimilar metal welds in Qinshan Nuclear Power Plant[J]. Nu-clear Power Engineering,2016(Suppl 2):7-9(in Chinese).

[13] 孙海涛,盛朝阳,高 晨,等. OVERLAY堆焊技术在核电设备维修中的应用[J]. 焊接,2015(9):53-56.

Sun Haitao,Sheng Zhaoyang,Gao Chen,et al. Ap-plication of OVERLAY welding technique to nuclear equipment maintenance and repairment[J]. Welding & Joining,2015(9):53-56(in Chinese).

[14] 操龙飞,徐 光,邓 鹏,等. 钢的热膨胀特性研究[J]. 北京科技大学学报,2014(5):639-643.

Cao Longfei,Xu Guang,Deng Peng,et al. Study on thermal expansion properties of steels[J]. Journal of University of Science and Technology Beijing,2014(5):639-643(in Chinese).

[15] 蒙玉勇,王建军,周 俐,等. 不同钢种导热系数随温度变化规律的研究[J]. 钢铁钒钛,2013,34(3):97-100.

Meng Yuyong,Wang Jianjun,Zhou Li,et al. Study on relationship between temperature and thermal con-ducti-vity in different kinds of steel[J]. Iron Steel Va-nadium Titanium,2013,34(3):97-100(in Chi-nese).

[16] Rong Y M,Mi G Y,Xu J J,et al. Laser penetration welding of ship steel EH36:A new heat source and application to predict residual stress considering mar-tensite phase transformation[J]. Marine Structures,2018,61:256-267.

[17] Peri? M,Tonkovi? Z,Rodi? A,et al. Numerical analysis and experimental investigation of welding re-sidual stresses and distortions in a T-joint fillet weld[J]. Materials & Design,2014,53:1052-1063.

[18] 武彦杰,覃寿同,赵冰清,等. 盾构机T形焊接结构的纯弯曲疲劳寿命研究[J]. 机械设计与制造,2012(8):124-125.

Wu Yanjie,Qin Shoutong,Zhao Bingqing,et al. Fa-tigue life study on pure bending of T-welded compo-nent of shield machine[J]. Machinery Design & Man-ufac-ture,2012(8):124-125(in Chinese).


备注/Memo

通信作者:程方杰,chfj@tju.edu.cn.